ABA SUPERSET-G

Description

Flexible thin bed mortar DESCRIPTION Thin-bed mortar for fixing ceramic tiles and vitrified tiles

ABA SUPERSET-G adheres to all solid, load-bearing, clean, dry and moist surfaces free of substances which can cause separation. Remove any coatings with inadequate bonding strength. Depressions of up to 5mm depth can be repaired with ABA SUPERSET-G the day before. Prime absorbent substrates such as calcium sulfate screeds, lightweight concrete, plasterboards and gypsum plasters, sandwich type and fibrous plasterboards with E.M.BOND. Allow the priming coat to dry for approx. 4 hours.

  • applicable for indoor and outdoor use
  • easy application
  • flexible
  • applicable for fixing vitrified tiles indoors
  • long open time
  • suitable for wet area application
  • available in white and grey colors

 

FIELD OF APPLICATION
For placing and fixing ceramic tile coverings indoors/outdoors, in wet areas and vitrified tiles indoors. Also suitable on heated screeds application. It is recommended to add 83 CC elastic emulsions for critical substrates such as young concrete and outdoor applications where high thermal stress is expected. ABA SUPERSET-G can also be used for the fixing of marble and natural stone not tending to discolor.
APPLICATION
Stir ABA SUPERSET-G into clean, clear water until it is completely free of lumps. Approx. 6.5 -7 l of water are needed to prepare 25 kg of ABA SUPERSET-G. Leave to mature for approx. 5 minutes and stir again. Apply the mortar according to the recognized rules of the thin-bed method. The skin formation time has always to be tested before applying the tiles. Apply by a notched spreader with suitable toothing to insure a contact area between mortar and tile of at least 65%. Fresh excess mortar can be removed with water, once hardened material can only be removed mechanically.

 

 

Base :   Polymer-modified cement combination with mineral fillers.
(Thin-bed mortar according to DIN EN 12004 C2T)
Bulk weight :   Approx. 1.3 g/cm3.
Mixing ratio :    Approx. 6.5-7 l of water for 25 kg of powder.
Maturing time :   5 minutes.
Application temperature :   +5°C to +40°C.
Application time :   Approx. 2 hours.
Open time :    Approx. 20 minutes.
Slip :   ≤ 0.10 mm.
Temperature resistance :   –30°C to +70°C.
Tensile adhesion strength :    ≥ 1.0 N/mm2.
Amount required (kg/m2) :   2.5-4.

 

PACKAGING
25 kg plastic bag.
STORAGE &SHELFLIFE
Approx. 12 months if stored in a tightly sealed container, in cool and dry conditions. Use product in opened containers as soon as possible.
TECHNICAL SERVICE
The ABADGARAN INTERNATIONAL GROUP Technical Department is available to assist you in the correct use of our products and its resources are at your disposal entirely without obligation.

 

  • ABA SUPERSET-G contains cement and reacts with water, producing an alkaline solution. Always protect skin and eyes. In case of contact, wash immediately with plenty of water. After eye contact seek medical advice. MSDS is available at ABADGARAN website.

 